DSC is an analytical instrument used to generate data regarding the thermal characteristics of a material by monitoring the change in heat flow of a sample material in comparison to a reference pan.? Properties measured can include melting temperature, crystallization temperature, glass transition temperature, percent crystallinity, information on curing, and more.?
![DSC](/research/sites/default/files/styles/max_width_480px/public/media/2021/05/picture2.png?itok=90OInqOD)
Manufacturer: | TA Instruments |
Model #:? |
Discovery DSC 250 |
Year of Manuf: | N/A |
Year Acquired: | 2019 |
Location:? | Parsons Hall N140 |
Specifications:
- Ability to run Modulated DSC
- Ultra High Purity Nitrogen Purge Gas
- -90°C to 725°C temperature range
- ±0.05°C Accuracy in Temperature
Principal scientist:?
?
?
The Knowledge Base contains forms, instruction?and training material, minutes, policies, tools and other resources to support your research efforts by topic area.
N140 Parsons Hall
Durham, NH 03824
Phone:?
Rates:
Non UNH Academic Rate:
$200.00/sample assisted
$80.00/sample unassisted
Industry rate:?
$200.00/sample assisted
$80.00/sample unassisted